Mar 29, 2024 Leave a message

High Temperature Resistant Seamless Tubes and Heat Resistant Grades

Why Heat Resistant Seamless Tubes Are Needed

High pressure boiler tubes belong to the seamless tube family, but they are ordered with much tighter requirements on the steel itself than ordinary seamless pipe. In service they are exposed simultaneously to high internal pressure, high metal temperature, oxidising flue gas and water vapour. Under those conditions the tube can lose section by oxidation and corrosion on the outside, scale and overheat on the inside, and creep under pressure, so the material must combine lasting strength, oxidation resistance, corrosion resistance and structural stability.

The tubes are used to build superheater tubes, reheater tubes, air guide tubes, main steam tubes and heat exchanger bundles for high pressure and ultra-high pressure boilers, as well as for process heat exchangers in refining, petrochemical, chemical and waste heat recovery service.

Grades for High Temperature and High Pressure Service

The austenitic stainless family provides the widest choice. Standard grades include 304, 304L, 304H, 304LN, 316L, 316H, 316Ti, 317, 317L, 321 and 321H; the stabilised grades 321H and 347H are used where the tube will operate in the sensitising range for long periods; and the high chromium grades 309S and 310S are selected where oxidation resistance at the highest metal temperatures is the governing requirement. Duplex grade S31803 is chosen where higher strength and better chloride stress corrosion resistance than the standard austenitic grades is needed, and 904L of the UNS N08904 class is used for severely corrosive process streams.

The ferritic and martensitic family covers 409, 409L, 410, 430, 436, 436L, 439, 439L and 444. These grades are used where thermal expansion must be kept low, for example in some heat exchanger and exhaust service, and where moderate corrosion resistance is sufficient.

Family Representative grades Typical reason for selection
Austenitic 304H, 316H, 321H, 347H Creep strength and structural stability at elevated metal temperature
High chromium austenitic 309S, 310S Oxidation resistance at the highest metal temperatures
Duplex S31803 Higher strength with improved chloride stress corrosion resistance
Ferritic and martensitic 409, 430, 436, 439, 444, 410 Low thermal expansion and moderate corrosion resistance

Standards for Seamless and Welded Supply

Seamless heat resistant tubes are commonly supplied to GB 13296, GB/T 14976 and GB/T 14975, to ASTM and ASME A213, A312, A269, A789 and A790, and to EN 10216-5 and DIN 17458. Welded tube for the same duties is supplied to GB/T 12770 and GB/T 12771, to ASTM and ASME A249, A312, A554, A778 and A789, and to EN 10217-7 and DIN 17457.

The standard selected determines which tests are mandatory. Specifications for boiler and heat exchanger tubing normally require chemical analysis, tensile testing, hardness testing, flattening and flaring tests, a hydrostatic or pneumatic test, and either an eddy current or an ultrasonic examination of the full length, with a grain size and intergranular corrosion check for the stabilised austenitic grades.

Applications

Superheater and reheater tubing in utility and industrial boilers.

Air guide tubes, main steam tubes and hot reheat lines in high pressure and ultra-high pressure units.

Heat exchanger tubes and U-bend bundles in refining, petrochemical and chemical plants.

Furnace and kiln internals, radiant tubes and high temperature process piping.

Waste heat recovery, incineration and exhaust systems where oxidation resistance is critical.

Selection and Processing Guidance

Selection starts from the design metal temperature, the flue gas or process atmosphere and the corrosivity of the stream. Within the austenitic family, choose the lowest alloy grade that satisfies the creep and oxidation requirement, because moving to a higher chromium or higher nickel grade raises both cost and weld sensitivity. Where the tube will be sensitised in service, specify a stabilised grade such as 321H or 347H, or a low carbon grade such as 304L or 316L.

For fabrication, stainless tube requires clean cutting and preparation, low heat input welding, controlled interpass temperature and, for the stabilised and duplex grades, strict attention to the consumable selection and to the heat input range, because too much heat input damages the duplex phase balance. Solution annealing after severe cold forming restores corrosion resistance, and a pickling and passivation treatment removes the oxide that forms on the heat affected zone.

FAQ

Q: What is the difference between a boiler tube and an ordinary seamless tube?
The manufacturing route is similar, but a boiler tube is ordered to a specification that controls the steel type much more strictly and imposes additional tests such as elevated temperature properties, flattening, flaring, grain size and non-destructive examination.

Q: Which grade is used where oxidation resistance at the highest temperature is required?
The high chromium austenitic grades 309S and 310S are selected for the highest metal temperature duties, because their chromium content provides the best scale resistance in oxidising atmospheres.

Q: When should a stabilised grade such as 321H or 347H be specified?
When the tube will remain in the sensitising temperature range for long periods during service, or when the welded joint will be exposed to a corrosive environment at elevated temperature.

Q: What are the equivalent standards for seamless supply?
The common seamless specifications are GB 13296, GB/T 14976, GB/T 14975, ASTM A213, A312, A269, A789 and A790, EN 10216-5 and DIN 17458.

Q: What tests should the mill certificate cover?
Chemical analysis, tensile and hardness results, flattening and flaring results, a pressure test, and a full length eddy current or ultrasonic examination, plus grain size and intergranular corrosion results where the grade is stabilised.

Q: Why is heat input controlled when welding duplex tube?
Duplex stainless steel depends on a balanced austenite and ferrite microstructure. Too high a heat input or too slow a cooling rate upsets that balance and reduces both toughness and corrosion resistance in the welded joint.