Welding joint surface
(1) Cracks, lack of fusion, pores, slag inclusions, and splashing are not allowed.
(2) There must be no undercut on the weld surface of pipes with a design temperature lower than -29 degrees, stainless steel and alloy steel pipes with a greater tendency to harden. The undercut depth of welds of pipes made of other materials should be greater than 0.5mm, the continuous undercut length should not be greater than 100mm, and the total undercut length on both sides of the weld should not be greater than 10% of the total length of the weld.
(3) The weld surface shall not be lower than the pipe surface. The weld reinforcement is , and shall not be greater than 3mm (it is the maximum width of the rear groove of the welded joint set).
(4) The misalignment of the welded joint should not be greater than 10% of the wall thickness and not greater than 2mm.
2. Surface non-destructive testing
Principles for selecting surface non-destructive testing methods for straight seam steel pipes: For steel pipes made of ferromagnetic materials, magnetic particle testing should be used; for steel pipes made of non-ferromagnetic materials, penetrant testing should be used.
For welded joints with a tendency of delayed cracking, the surface non-destructive inspection should be carried out after the welding has cooled for a certain period of time; for welded joints with a tendency of reheat cracking, the surface non-destructive inspection should be carried out once after welding and after heat treatment.
The application of surface non-destructive testing is carried out in accordance with standard requirements. Its detection objects and application occasions are generally as follows:
(1) Quality inspection of the outer surface of pipe materials.
(2) Detection of surface defects of important butt welds.
(3) Detection of important fillet weld surface defects.
(4) Surface defect detection of welded joints of important socket welds and crossover tee branches.
(5) Detection of surface defects after pipe bending.
(6) Groove detection of welded joints with large material quenching tendency.
(7) Detection of grooves of non-austenitic stainless steel pipes with design temperature lower than or equal to minus 29 degrees Celsius.
(8) Inspection after root cleaning of welds requiring root cleaning for double-sided weldments
(9) When using oxyacetylene flame to cut welding fixtures on alloy pipes with a tendency to harden, defect detection of the grinding parts.