What ASTM A691 Pipe Is
ASTM A691 is the standard specification for carbon and alloy steel pipe made by electric-fusion welding for high-pressure service at high temperatures. It is not a general line pipe specification: A691 is written around the welding procedure and the thermal treatment of the finished pipe, so it controls the base plate, the filler metal, the quality of the longitudinal seam and the final condition of the delivered length.
Pipe is normally produced from plate that is cold or hot formed into a cylinder and joined with a longitudinal seam welded from both sides. Depending on the grade and class, the seam may be completed with a filler metal that matches the base metal, with a higher-alloy filler metal, or without filler metal at all. Wall thickness is usually greater than that of standard line pipe, because the intended service combines pressure with elevated temperature.
How the Grade and Class System Works
A691 grades are identified by nominal alloy content rather than by a simple strength number. Common grades fall in the low-chrome and chrome-molybdenum families, for example 1/2 Cr, 1 Cr, 1-1/4 Cr, 2-1/4 Cr and 5 Cr. The alloy level governs the elevated-temperature strength and the oxidation and hydrogen resistance of the pipe, and it also determines the welding consumables and the preheat that the fabricator must apply.
Each grade is supplied in several classes. The class fixes two variables: the analysis of the filler metal used for the seam, and the heat treatment the pipe receives after welding. As a result, two pipes carrying the same grade can differ in tensile properties and in the amount of weld examination that applies. The complete grade-and-class designation therefore has to be quoted in full on the purchase order, and the marking on each length has to carry it as well.
Specification Overview
| Item | Requirement |
|---|---|
| Standard | ASTM A691, electric-fusion-welded carbon and alloy steel pipe for high-pressure service at high temperatures |
| Product form | Plate formed to a cylinder with a longitudinal double-welded seam |
| Grades | Defined by nominal alloy content, such as 1/2 Cr, 1 Cr, 1-1/4 Cr, 2-1/4 Cr and 5 Cr |
| Classes | Two-part designation fixing filler metal analysis and heat treatment |
| Heat treatment | Normalizing, normalizing and tempering, or stress relieving, as required for the grade and class |
| Ends | Plain, beveled or threaded, according to the order |
| Testing | Hydrostatic test or non-destructive electric test, plus weld seam examination where supplementary requirements are ordered |
| Marking | Standard designation, grade and class, size, wall thickness, heat number and length |
Advantages in Service
The main advantage of A691 pipe is that it holds its strength at temperature. Low-alloy chrome and chrome-molybdenum steels retain tensile and creep resistance far better than plain carbon steel, so a thinner wall can carry the same design pressure in a hot circuit, which reduces weight, welding volume and support cost.
The second advantage is the welded construction itself. Electric-fusion welding from plate gives a uniform wall, a controlled seam and the possibility of a heavier section than a comparable seamless product. The third is inspection transparency: because the seam is made in the shop, it can be radiographed or ultrasonically examined before dispatch, and the heat treatment given to the finished pipe is recorded against the heat number.
Corrosion behaviour in hot process streams is also better than that of carbon steel, particularly where sulphidic or oxidising conditions are present. The alloy content is not a substitute for a stainless or nickel alloy in strongly aggressive service, but it extends life considerably in the temperature range where carbon steel begins to scale and thin.
Typical Application Fields
Refinery process piping: hydrotreater, hydrocracker, catalytic reformer and delayed coker circuits where hydrogen partial pressure and temperature are both high.
Power generation: high-temperature steam headers, hot reheat lines and main steam piping in fossil-fired and combined-cycle plants.
Petrochemical plants: reactor interconnecting lines, furnace transfer lines and heat exchanger shells working above the creep range of carbon steel.
Chemical processing: pressure vessels and piping handling hot gases, process condensate and mildly corrosive media.
Heat recovery and industrial steam distribution: hot-oil and steam mains where thermal cycling requires stable mechanical properties.
Ordering, Welding and Inspection Points
The grade and class must be stated together, with size, nominal wall thickness, length, end finish, heat treatment condition and any supplementary requirements such as additional radiographic examination of the seam or impact testing at a stated temperature. Because the seam and the base plate are both covered by the standard, the mill test certificate reports the plate analysis, the weld procedure, the heat treatment and the mechanical results for each heat.
For fabrication, chrome-molybdenum grades require controlled preheat, interpass temperature limits and, after welding, an approved post-weld heat treatment in accordance with the governing construction code, for example ASME B31.3. Consumables must be selected for the actual grade and class, not simply for the nominal alloy level, because hydrogen cracking resistance depends on the combination of alloy, section thickness and cooling rate. Low-hydrogen practice, dry consumable storage and careful control of fit-up are standard requirements.
On receipt, verify the marking against the certificate, check the seam for uniformity and weld reinforcement, measure ovality and wall thickness at several positions, and confirm that the specified heat treatment has been applied to the finished pipe rather than to the plate alone.
FAQ
Q: What does the class number in an A691 designation mean?
The class identifies the filler metal used for the longitudinal seam together with the heat treatment applied to the completed pipe. It must always be quoted with the grade, because it changes both the mechanical properties and the examination requirements.
Q: Is ASTM A691 pipe seamless or welded?
It is welded, and specifically electric-fusion welded from formed plate with a longitudinal seam. The seam is normally welded from both sides, and may be produced with or without filler metal depending on the grade and class.
Q: Which grades are most common in refinery service?
The chrome and chrome-molybdenum grades in the range from 1/2 Cr up to 2-1/4 Cr dominate hot process piping, while higher-alloy grades are chosen where temperature, hydrogen partial pressure or oxidation resistance is more demanding.
Q: Does A691 pipe need post-weld heat treatment after field welding?
Yes for the alloy grades in most applications. The construction code that governs the plant, such as ASME B31.3, sets the thickness and material conditions under which post-weld heat treatment is mandatory, and the procedure must be qualified for the actual grade and class.
Q: How is the pipe tested before shipment?
Each length is subjected to a hydrostatic or non-destructive electric test as specified, and the longitudinal seam is examined radiographically or ultrasonically when supplementary requirements are ordered. Mechanical testing is performed on the heat and on the finished pipe as the standard provides.
Q: Can A691 pipe be used in sour service?
The selection depends on the environment, not on the specification alone. Where wet hydrogen sulphide is present, the hardness, chemistry and stress state must be assessed against the recognized sour-service requirements, and a lower-strength or controlled-hardness condition may be needed.