ASTM A179 ASME SA179 Seamless Heat Exchanger Tube

Heat Treatment of ASTM A179,ASME SA179
ASTM A179,ASME SA179 steel tubes are heat treated after the final cold draw pass at a temperature of 1200°F [650°C] or higher.
Chemical Composition of ASTM A179,ASME SA179 Seamless Heat-Exchanger and Condenser Tubes

Material Chemical Composition(%)
C Si Mn P S
ASTM A179 0.06-0.18 ≤ 0.25 0.27-0.63 ≤0.035 ≤0.035

Mechanical Propertie of ASTM A179,ASME SA179 Seamless Heat-Exchanger and Condenser Tubes

Grade ASTM A179
Tensile Strength(MPa) ≥325
Yield Strength(MPa) ≥180
Elongation,% ≥35
Hardness, HRB ≤72

Note -Tubing smaller in outside diameter and having a thinner wall than indicated in this specification is available. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] in outside diameter or with a wall thickness under 0.015 in. [0.4 mm].
The dimensional tolerances of ASTM A179,ASME SA179 Seamless Heat-Exchanger and Condenser Tubes
Tolerances of Wall Thickness

Outside
Diameter,
in. [mm]
Wall Thickness, %
0.095[2.4] and Under Over 0.095 to 0.150
[2.4 to 3.8], incl
Over 0.150 to 0.180
[3.8 to 4.6], incl
Over 0.180,[4.6]
Over Under Over Under Over Under Over Under
Seamless, Cold-Finished Tubes
  Over Under
1 1 ⁄ 2 [38.1] and under 20 0
Over 1 1 ⁄ 2 [38.1] 22 0

Tolerances of Outside Diameter

Outside Diameter,in. [mm] Permissible Variations, in. [mm]
Over Under
Under 1 [25.4] 0.004 [0.1] 0.004 [0.1]
1 to 1 1 ⁄ 2 [25.4 to 38.1], incl 0.006 [0.15] 0.006 [0.15]
Over 1 1 ⁄ 2 to 2 [38.1 to 50.8], excl 0.008 [0.2] 0.008 [0.2]
2 to 2 1 ⁄ 2 [50.8 to 63.5], excl 0.010 [0.25] 0.010 [0.25]
2 1 ⁄ 2 to 3 [63.5 to 76.2], excl 0.012 [0.3] 0.012 [0.3]
3 to 4 [76.2 to 101.6], incl 0.015 [0.38] 0.015 [0.38]
Over 4 to 7 1 ⁄ 2 [101.6 to 190.5], incl 0.015 [0.38] 0.025 [0.64]
Over 7 1 ⁄ 2 to 9 [190.5 to 228.6], incl 0.015 [0.38] 0.045 [1.14]

info-1000-800

 